Excellent anti-aging performance, service life up to 50 years.
- high extension rate, high tensile strength, small size changes at heat treatment.
- Good plant roots penetrability resistance and can be made waterproofing layer of planting roof.
- Special modified molecular structure ,effectively resolving the current domestic and foreign glue joint problem .
- Good low temperature flexibility, and good performance of adapting to ambient temperature changes.
- Convenient application , solid joint, no environment pollution.
- chemical corrosion Resistance, can be used for special occasions.
- Convenient maintainance, low cost.
- Convenient for dealing with details.
- Good Anti-perforated.
TESTED PROPERTY | TEST METHOD | UNIT ENGLISH METRIC | VALUE ENGLISH(METRIC | |
45mil | 60mil | |||
Color | Black | Black | ||
Thickness, nominal ±10% | ASTM D 5199 | mil (mm) | 45 (1.14) | 60 (1.52) |
TENSILE PROPERTIES | ||||
Break Strength | ASTM D 882 | lb/in (kN/m) | 50 (9) | 65 (11.4) |
Break Elongation | ASTM D 882 | % | 500 | 500 |
Tear Resistance lbf/in (kN/m) | ASTM D 1004 | lbs (N) | 9 (40) | 12 (50) |
Puncture Resistance | ASTM D 4883 | lbs (N) | 35 (150) | 45 (190) |
Brittleness Temperature | ASTM D 746 | ˚F (˚C) | -49(-45) | -49(-45) |
Water Vapor Permeance Max. Perms | ASTM E 96 (Proc B or W) | 2.0 | 2.0 | |
Resistance to Water Absorption % change in mass max. after 7 days immersion @ 170˚F (65˚C) | ASTM D 471 | +8.0 -2.0 | +8.0 -2.0 | |
Resistance to Heat Aging (Properties after 170 hrs @ 212˚F (100˚C) 1. Tensile Break Strength 2. Elongation, ultimate min. | ASTM D 882 | % | 90 75 | 90 75 |
Multiaxial Elongation | ASTM D 5617 | % | 100 | 100 |
Dimensional Stability | ASTM D 1204 | % | 0.75 | 0.75 |
Ozone Resistance Condition after exposure to 100pphm ozone in air for 168 hrs @ 140˚F (40˚C) (Sample under 50% strain) | ASTM D 1149 | No Cracks | No Cracks | |
Resistance to outdoor (Ultraviolet) Weathering , Xenon-Arc, 4000 hr exposure @ 70˚F (176˚F) Black panel temperature, visual condition | ASTM G 26 | No Cracks | No Cracks | |
Toxicity to Fish | ASTM E 729 (96) Modified | Passes | Passes | |
Shore A Durometer | ASTM D 2240 | 65±10 | 65±10 | |
This data is provided for informational purposes only. Trump Eco makes no warranties as to the suitability or the fitness for a specific use or merchantability of the products referred to, no guarantee of satisfactory results from reliance upon contained information or recommendations and disclaims all liability from resulting loss or damage. This information is subject to change without notice, |
-
Professional Team
Over 30 years experience, we are always able to find the best solution for you. -
Quick Response
24*7 service. You will always get answers in 6 hours. -
Trust
We promise to supply products as per sample and your requirement,not cheat any client. -
One Stop Solution
From the beginning to end, we take care of every step in your project. -
Free Sample and High Customization
Sample will be free for you, and products liner as per the sizes of your roof and pond. -
Free Value-added Service
Finding you the solution is the first step, more service (technical support, construction guidance etc) will supply to you soon.
- Irrigation ponds, canals, reservoirs, & ditches.
- Agricultural applications.
- Liners & covers.
- Golf courses & decorative ponds.
- Earthed-in water dam impervious liner layer.
- Sub zero installations.